Bluing is a type of dye that was used to check the fit of parts. Basically a very fine layer would be spread on a gauge or mating part and then fit to the gauge or other mating part. After rubbing or twisting these parts, depending on what they were, the bluing would either be evenly transferred to the mating part or rubbed away from the part being tried for fit.

I used it quite often while running grinders to make sure various tapers fit the appropriate guage and to determine if the angle was off, which way and by how much it was off. If all the bluing was rubbed off along the entire length of the part I was grinding then I knew I had the right angle.

I had also seen it used quite often when machine ways were being scraped for a flat fit.

A more formal term for it was Engineer’s Blue

Since this dye was not water soluble it was very sticky and would stain anything it came in contact with. It was very difficult to get off and often required the use of an oil based solvent to get it off your skin. If you tried to wipe it off or wash it off with soap and water it would just smear and spread even more.

Thus “getting blued” was not a fun experience.